Abstract

RED X-11 is a heat treatable aluminum alloy of the silicon-copper-magnesium type. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and joining. Filing Code: Al-86. Producer or source: Apex Smelting Company.