Abstract
HY-TEN MC is an electric furnace oil hardening alloy steel having good depth hardenability and desirable non-deforming characteristics. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-90. Producer or source: Wheelock, Lovejoy & Company Inc..