HI TENSILE is an aluminum-zinc-magnesium casting alloy having high strength without heat treatment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-83. Producer or source: R. Lavin & Sons Inc..