Zilloy 15 is a zinc-base alloy strip recommended for drawn or mildly formed parts requiring maximum stiffness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as casting, forming, heat treating, and joining. Filing Code: Zn-6. Producer or source: New Jersey Zinc Company.