Abstract
WEARPACT is a low alloy cast steel combining wear and impact resistance to a high degree. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness and fatigue. It also includes information on low temperature performance as well as casting, heat treating, machining, and joining. Filing Code: SA-79. Producer or source: American Steel Foundries.