Deutsche Edelstahlwerke Cryodur 2362 is a high-carbon, chromium-molybdenum-vanadium alloy cold-work tool steel with high tempering resistance. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fatigue. It also includes information on wear resistance as well as forming and heat treating. Filing Code: TS-840. Producer or source: Deutsche Edelstahlwerke Specialty Steel GmbH.