Aubert & Duval Ti17 (UNS R58650) is a “beta-rich” alpha-beta titanium-aluminum-molybdenum-chromium-zirconium-tin alloy. This alloy has higher tensile and creep strengths than Ti-6Al-4V. While its hardenability is similar to that of other beta alloys, Aubert & Duval Ti17 has a lower density and a higher modulus than most other beta titanium alloys. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ti-195. Producer or source: Aubert & Duval S.A.