Elgiloy CP Titanium Grade 2 (Ti 40) is an unalloyed commercially pure titanium. It is widely used for applications requiring a combination of moderate strength, high ductility, excellent corrosion resistance, and good weldability. This grade can be used in the temperature range –184 to 540 °C (–300 to 1000 °F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-194. Producer or source: Elgiloy Specialty Metals.