Böhler L090 is a wrought, precipitation-hardenable, nickel-chromium-cobalt alloy that is strengthened by additions of titanium and aluminum. It has been developed as an age-hardenable creep resisting alloy for service at temperatures up to 900 °C (1650 °F). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming and heat treating. Filing Code: Ni-784. Producer or source: voestalpine Böhler Edelstahl GmbH & Co KG.