1025, C25, C25E, and C25R are wrought low-carbon (carbon = 0.22–0.29%) non-alloy steels that are used in the normalized, cold worked, or quenched and tempered condition. 1025, C25E, and C25R may also be nitrided or nitrocarburized. These steels are widely used for small, moderately stressed parts that require higher strength levels than can be achieved by the lower carbon grades, and also for applications that require a combination of moderate strength, high toughness, and good fabrication characteristics. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming and heat treating. Filing Code: CS-252. Producer or source: Heat Treater's Guide.