Elgiloy CP Titanium Grade 1 / Ti 25 is an unalloyed commercially pure titanium. It has the highest purity, lowest strength, and best ductility and formability of the four ASTM unalloyed titanium grades. This grade can be used in the temperature range -184 to 540 °C (-300 to 1000 °F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-193. Producer or source: Elgiloy Specialty Metals.