Abstract
Aubert & Duval TA6V ELI (UNS R56401) is an alpha-beta, titanium-aluminum-vanadium alloy that is normally used in the annealed condition. It is a purer version of Aubert & Duval TA6V, with a lower oxygen and iron content. Aubert & Duval TA6V ELI is especially popular due to its ductility at cryogenic temperatures and its excellent biocompatibility with the human body. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-192. Producer or source: Aubert & Duval S.A.