Abstract
Uddeholm Corrax for AM is a stainless steel developed for additive manufacturing. Its unique set of properties makes it a choice for tools where superior corrosion resistance combined with high hardness is needed. These properties make it suitable for tools for plastic molds, including for demanding applications such as molds for medical parts, parts made of corrosive plastics, and parts made of rubber. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength. It also includes information on corrosion resistance as well as forming, heat treating, surface treatment, and powder metal forms. Filing Code: SS-1358. Producer or source: Uddeholms AB.