Austral Wright Alloy B25 (UNS C17200) is a wrought beryllium copper alloy. It provides the highest strength of any copper alloy, with electrical conductivity considerably greater than that of other high-strength copper alloys. Since it is heat treated after forming, it provides excellent formability and ductility. This alloy features good stress relaxation resistance and high fatigue strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Cu-943. Producer or source: Austral Wright Metals.