Deutsche Edelstahlwerke Cryodur 2721 is a medium-carbon, nickel-chromium alloy cold-work tool steel. This oil hardening type cold work tool steel offers a combination of high hardness, good wear resistance, high toughness, and good machinability. This datasheet provides information on composition, physical properties, microstructure, hardness, and elasticity. It also includes information on forming and heat treating. Filing Code: TS-839. Producer or source: Deutsche Edelstahlwerke Specialty Steel.