Böhler K329 is a chromium-molybdenum-vanadium alloy cold-work tool steel. It is characterized by excellent toughness and good wear resistance. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming and heat treating. Filing Code: TS-829. Producer or source: voestalpine Böhler Edelstahl GmbH & Co KG.