BÖHLER K306 is a chromium-molybdenum-vanadium, alloy cold-work tool steel that is characterized by excellent toughness and wear resistance, and high retention of hardness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, and machining. Filing Code: TS-827. Producer or source: voestalpine Böhler Edelstahl GmbH & Co KG.