Mueller Brass C11000 (electrolytic tough pitch copper) is an electrolytically refined, high conductivity copper that contains a minimum of 99.90% copper and a controlled amount of oxygen in the form of Cu2O. It has a minimum electrical conductivity of 100% IACS. Electrolytic tough pitch copper (C11000) is the most widely used grade of copper in electrical applications all over the world and represents over half of global copper use. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: Cu-931. Producer or source: Mueller Brass Company.