Uddeholm Unimax is a high-hardness chromium-molybdenum-vanadium alloy hot-work tool steel that provides high wear resistance at elevated temperatures. It performs very well in precision forging and hot stamping. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on heat treating and machining. Filing Code: TS-826. Producer or source: Uddeholms AB.