1025, 1026, C25, C25E, and C25R are wrought low-carbon non-alloy steels that are used in the normalized, cold worked, or quenched and tempered condition. These steels are widely used for small, moderately stressed parts that require higher strength levels than can be achieved by the lower carbon grades, and also for applications that require a combination of moderate strength, good toughness, and good fabrication characteristics. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CS-221. Producer or source: Data Survey.