Abstract
1033 and S33C are wrought medium-carbon non-alloy steels that are used in the normalized, cold worked, or quenched and tempered condition. 1033 and S33C may also be flame or induction hardened. These steels are widely used for small, moderately stressed parts that require higher strength levels than can be achieved by the lower carbon grades, and also for applications where a combination of moderate strength and good toughness is required. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CS-236. Producer or source: Data Survey.