1017 and S17C are wrought low-carbon (C = 0.15–0.20%) non-alloy steels that are used in the as rolled, normalized, or cold worked condition. These steels are widely used for lightly and moderately stressed parts that require higher strength levels than can be achieved by the lower carbon grades, and also for applications where a combination of low-to-medium strength, excellent cold formability, and excellent weldability are required. They may also be used in the carburized or carbonitrided, and subsequently quench hardened and tempered condition for parts requiring a hard, wear-resistant surface, but with little need for increased mechanical properties in the core. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CS-234. Producer or source: Data Survey.