Deutsche Edelstahlwerke Cryodur 2008 is a high-carbon, chromium-vanadium alloy cold-work tool steel that is suitable for applications requiring a combination of high strength, good toughness, and good wear resistance. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on wear resistance as well as forming, heat treating, and machining. Filing Code: TS-832. Producer or source: Deutsche Edelstahlwerke Specialty Steel.