Abstract
Aurubis Cu-DLP is a phosphorus-deoxidized copper that contains a minimum of 99.90% copper and a small amount of residual phosphorus. Owing to the presence of residual phosphorus, the electrical conductivity of Aurubis Cu-DLP is lower than that of the high-conductivity and oxygen-free coppers (Cu-ETP, Cu-FRHC, and Cu-OF). Its conductivity is, however, higher than that of Cu-DHP and Cu-HCP. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-928. Producer or source: Aurubis AG.