Abstract

Deutsche Edelstahlwerke Cryodur 2242 is a medium-carbon, chromium-vanadium alloy cold-work tool steel that has medium hardenability and is suitable for applications requiring a combination of high strength, high toughness, and good wear resistance. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-816. Producer or source: Deutsche Edelstahlwerke Specialty Steel.