Abstract

Schmelzmetall Hovadur CCB is a heat-treatable, copper-cobalt-beryllium alloy. In the solution heat treated and artificially aged condition, this alloy combines good mechanical strength and excellent ductility as well as high softening temperature with good thermal and electrical conductivity. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-920. Producer or source: Schmelzmetall AG.