L. Klein Titan Grade 2 is an unalloyed, commercially pure titanium grade. It is the most widely used commercially pure titanium grade. It offers a combination of moderate strength and good ductility, with outstanding corrosion resistance in many challenging service environments. L. Klein Titan Grade 2 can operate in continuous service up to 425 °C (800 °F) and in intermittent service up to 540 °C (1005 °F). This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance and wear resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-177. Producer or source: L. Klein SA.