Abstract
ATI 20-25+Nb is an austenitic stainless steel intended primarily for elevated-temperature service. This alloy fills a performance gap between conventional heat-resistant stainless steels and nickel-base superalloys, providing high performance with an economical composition. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SS-1331. Producer or source: ATI.