Abstract

ATI 35N is a wrought, multi-phase Co-Ni-Cr-Mo alloy that can be heat treated to achieve very high strength, while maintaining excellent toughness, ductility, and corrosion resistance. To achieve tensile strength levels of 1795 to 2070 MPa (260 to 300 ksi), the alloy is cold worked and then precipitation hardened. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Co-133. Producer or source: ATI.