Abstract

Greek Ascoloy is a heat resisting alloy steel offering satisfactory resistance to temperatures slightly above 1000 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-78. Producer or source: Firth Sterling Inc..