Abstract

MEEHANITE GB is a high strength iron casting having high damping capacity, self-lubricating properties, and good machinability. It combines the good properties of both cast iron and steel. Applications include machine tools, gears, shafts, housings, lathe beds, bases, pistons, crankshafts, camshafts, and general engineering castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on high temperature performance as well as heat treating and joining. Filing Code: CI-22. Producer or source: Meehanite Metal Corporation.