Aluminum 5456 is an aluminum-magnesium alloy suitable for structural welding applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on forming, heat treating, machining, and joining. Filing Code: Al-70. Producer or source: Aluminum Company of America.