Abstract
AIRLOY is a non-deforming, air-hardening cold work die steel. It has good wearing qualities, strength and toughness. This datasheet provides information on composition and hardness as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-73. Producer or source: Allegheny Ludlum Corporation.