Abstract

D-H No. 245 is a nickel-base alloy with extraordinary oxidation resistance at elevated temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance. Filing Code: Ni-43. Producer or source: Driver-Harris Company.