BERALOY is a beryllium-copper alloy supplied in two grades: Beraloy A and Beraloy D. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-65. Producer or source: Wilbur B. Driver Company.