APEX 36 is a high silicon, aluminum die casting alloy having high fluidity, excellent castability and good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness and fatigue. It also includes information on high temperature performance as well as casting and machining. Filing Code: Al-66. Producer or source: Apex Smelting Company.