Abstract

NI-TENSYLIRON is a nickel cast iron with tensile strength greater than 50,000 psi. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness and fatigue. It also includes information on machining and joining. Filing Code: CI-20. Producer or source: International Nickel Company Inc..