Abstract

ALUMINUM 6066 is a heat treatable aluminum alloy having good strength and excellent fabricating characteristics. It was developed as an extrusion alloy. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-63. Producer or source: Harvey Aluminum Company.