VASCO-WCC is a hot work die steel having improved mechanical properties at elevated temperatures and is highly resistant to heat checking. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, and joining. Filing Code: TS-77. Producer or source: Vanadium Alloys Steel Corporation.