MALLEABLE IRON is a tough, malleable, shock-resisting cast iron. It has good corrosion resistance and excellent stability at elevated temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as casting, forming, heat treating, machining, and joining. Filing Code: CI-23. Producer or source: Malleable iron foundries.