Abstract

AMBRALOY-928 is a copper-aluminum alloy having high strength, hardness and excellent resistance to general corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: Cu-69. Producer or source: American Brass Company.