Abstract

Zapp Ergste 1.4028YN is a medium-carbon, 13% Cr, martensitic stainless steel that is designed for medical applications requiring high strength and hardness along with good corrosion resistance in moderately corrosive environments. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1326. Producer or Source: Zapp AG.

This content is only available as a PDF.
You do not currently have access to this content.