Raffmetal EN AB-Al Si2MgTi is a heat-treatable, Al-Si-Mg-Mn-Ti casting alloy casting alloy in ingot form for remelting. It is used extensively for producing sand and permanent mold castings for applications requiring a combination of good strength and shock resistance, good corrosion resistance, and suitability for decorative anodizing and welding. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, and machining. Filing Code: Al-467. Producer or Source: Raffmetal S.p.A.