Abstract

ATI 75 (UNS N06075) is a nickel-chromium alloy with controlled additions of titanium and carbon; it derives its high temperature strength essentially from solid solution strengthening. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, and joining. Filing Code: Ni-761. Producer or source: ATI.