Abstract

ATI 3-2.5 is a Titanium-3Aluminum-2.5Vanadium alloy that has higher strength than unalloyed titanium and is much more amenable to cold working than Ti-6Al-4V. This near-alpha, alpha-beta alloy is generally used in the annealed or cold-worked and stress-relieved conditions. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-166. Producer or source: ATI.