Abstract

Uddeholm Formax is a high-manganese, low-carbon, non-alloy cold work tool steel that is primarily used in the non-heat-treated condition. For special applications it is used in the case-hardened condition. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, and joining. Filing Code: TS-793. Producer or source: Uddeholms AB.