Abstract

Zapp TiAl6V4 is an alpha-beta titanium alloy that is used in the annealed or solution heat treated and aged condition for applications requiring high strength, relatively low weight, and excellent corrosion resistance. It is typically used in the low to moderate temperature range (up to about 400 °C, or 750 °F). Ti-6Al-4V is the most widely used titanium alloy, accounting for more than 50% of the total titanium used. The aerospace industry accounts for more than 80% of this usage. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-173. Producer or source: Zapp AG.