Lucefin Group 20NiCrMo2-2 and 20NiCrMoS2-2 are low-carbon, Ni-Cr-Mo, alloy case-hardening steels that are used in the carburized or carbonitrided, and subsequently quench hardened and tempered, condition. These steels are, in general, used for medium-size case-hardened parts requiring high fatigue strength and wear resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, and joining. Filing Code: SA-866. Producer or source: Lucefin S.p.A..