Abstract

ATI 6230 is a solid-solution strengthened, corrosion and heat-resistant, Ni-Cr-W-Mo-Al-La alloy. It is typically used for parts requiring good resistance to oxidizing environments up to 1150 °C (2100 °F) and relatively high strength up to 980 °C (1800 °F); however, usage is not limited to such applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: Ni-765. Producer or source: ATI.