Abstract

Wieland Duro Tantalum is unalloyed tantalum that is produced from powder metallurgy consolidated ingots. It is a versatile refractory metal that is used in demanding applications requiring resistance to high temperature and corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on low and high temperature performance as well as machining and joining. Filing Code: Ta-14. Producer or source: Wieland Duro GmbH.